My old painter told me to quit blocking primer with 220 and it saved my last two jobs
Two jobs ago I had a truck bed come back with sand scratch swelling after 3 weeks. I asked Ray, the guy who trained me back in Toledo, what I did wrong. He looked at my grit sheet and laughed. Told me I was polishing primer instead of cutting it, and that 220 on a DA just heats the surface and smears it instead of leveling. He said step down to 180 on a soft pad, then 320 wet before sealer, and quit chasing a mirror finish on primer. Switched to that on the next two collision jobs and no comebacks. Curious what grit you all finish primer at before sealer, especially on those big flat door skins.